Ultra-low viscosity CMC is a special form of carboxymethyl cellulose sodium (CMC-Na), featuring low viscosity, good water solubility, and strong stability. It is widely used in various fields. The relevant information is as follows:
Characteristics: It has a lower molecular weight, better solubility and fluidity, and can rapidly dissolve in water to form a colloidal solution. At the same time, it also has good stability, can maintain a dissolved state under different temperatures and pH conditions, and can effectively emulsify and disperse in liquids.
Ultra-low viscosity CMC, due to its unique properties, has extensive applications in multiple fields, as follows:
Paper industry: used in coating paper and paperboard production, as a rheological control agent, water retention agent, film-forming agent, and auxiliary adhesive for coatings, it can increase the solid content of the coating and maintain good rheological properties, improve the adaptability of paper printing, and is suitable for high-speed coating production processes.
Textile industry: used as a sizing agent and thickener for printing pastes, helps improve the printing quality of textiles, and can also be used for the stiffening treatment of textiles to enhance the adhesion and wear resistance of fibers.

module title
Lorem ipsum dolor sit amet consectetur
Raw material pretreatment:
Select high-purity cellulose raw materials, after grinding and screening, treat them with an alkaline solution (usually NaOH solution) for alkalization to relax the cellulose molecular chains and generate alkyl cellulose (cellulose sodium), creating conditions for the subsequent etherification reaction. The alkalization conditions (such as temperature, alkali concentration, and time) need to be precisely controlled to avoid excessive degradation or uneven reactions.
Etherification reaction:
alkyl cellulose reacts with an etherifying agent (such as sodium chloroacetate) at a certain temperature (usually 50-70°C) and solvent (such as ethanol-water mixture) to introduce carboxymethyl groups (-CH₂COONa). This step is crucial for controlling viscosity: by adjusting the dosage of etherifying agent, reaction time, temperature, etc., the degree of substitution and molecular weight can be controlled - a lower molecular weight and moderate substitution degree (usually 0.5-1.2) can achieve ultra-low viscosity characteristics.
Neutralization and washing:
After the reaction, neutralize the excess alkali with acid (such as hydrochloric acid) to make the pH value of the product neutral. Then, through washing (commonly with ethanol solution), remove unreacted impurities, salts, and by-products to improve product purity, avoiding residual impurities affecting subsequent applications (such as in the food and medicine fields where purity is extremely high).
Drying and grinding:
The wet product after the reaction is dried (such as hot air drying) to remove moisture, control the moisture content below 10%, and then ground into a certain particle size powder to obtain the ultra-low viscosity CMC product. The drying temperature needs to be moderate to prevent product degradation or color changes caused by high temperatures.
Post-treatment:
Depending on the application requirements, some products may undergo further refinement (such as decolorization, impurity removal) or modification treatment (such as cross-linking, compounding) to optimize their dispersibility, salt resistance, and other properties to meet the requirements of specific fields (such as lithium batteries, medicine).
special process:
Second chemical viscosity reduction. The core of the entire process lies in precisely controlling the raw material pretreatment and etherification reaction conditions to achieve effective regulation of molecular weight and viscosity, while ensuring key indicators such as water solubility and stability.
Production Process
Raw Material Control - Strictly select raw materials
Use high-purity cellulose (such as silver star wood pulp), requiring high cellulose content (usually ≥ 95%) and few impurities (such as low ash content, low metal ion content), to avoid impurities affecting subsequent reactions and product purity. - Standardized Raw Material Pre-treatment: The particle size of the crushed cellulose should be uniform. Before alkalization, large particles should be removed through screening to ensure sufficient and consistent alkalization reaction.
01
Reaction Process Parameter Control - Alkalization Stage:
Precisely control the concentration of alkaline solution (such as NaOH concentration 15%-20%), temperature (20-30℃), and reaction time (1-2 hours), to avoid excessive alkalization that leads to uneven cellulose degradation and affects the subsequent etherification efficiency. - Etherification Stage: By adjusting the dosage of etherifying agent (sodium chloroacetate), reaction temperature (50-70℃), reaction time, and solvent ratio, strictly control the substitution degree (usually 0.5-1.2) and molecular weight - Low substitution degree will result in poor water solubility, while high substitution degree may increase viscosity; the molecular weight needs to be controlled through reaction conditions to the target range to ensure that the final product viscosity meets the standard (such as viscosity of 1% water solution < 50 mPa·s).
02
Purification and Washing Control - Neutralization Precision:
When neutralizing excess alkaline with hydrochloric acid, strictly control the pH value within 6.5-7.5 to avoid strong acidity, causing product degradation or residual alkalinity affecting stability. - Multi-stage Washing: Use a mixture of ethanol and water for multiple washes to remove unreacted salts, residual etherifying agents, and by-products, ensuring product purity (such as food grade purity ≥ 99%, higher for pharmaceutical grade), and testing the conductivity of the washing liquid to ensure it meets the standard before stopping the washing.
03
Drying and Post-Treatment Control - Drying Conditions:
Control the drying temperature (60-80℃) and time to avoid high temperature causing product degradation or discoloration, ensuring moisture content < 10%, preventing caking or mold growth. - Particle Size of Crushing: Control the particle size of the finished product (such as 80-200 mesh) according to application requirements to ensure product dispersibility and dissolution speed.
04
Finished Product Testing and Quality Traceability - Key Indicator Testing:
Before leaving the factory, test viscosity (1% water solution, 25℃), substitution degree, purity (ash content, heavy metals), pH value, moisture, etc., to ensure compliance with industry standards. - Batch Management: Record raw material sources, reaction parameters, and test results to achieve quality traceability, facilitating timely problem identification. Through the above measures, ultra-low viscosity CMC can meet the strict requirements of various fields such as food, medicine, and lithium batteries in terms of viscosity stability, purity, and applicability.
05
Physical and chemical indicators
|
Appearance |
White or slightly yellow powder particles |
|
PH |
7.5-8.5 |
|
D.S |
8.0-9.0 |
|
Moisture |
7-9 |
|
Viscosity |
<25 |
|
Purity |
>90 |
Product Features
① Excellent solubility, can be dissolved evenly by stirring at room temperature.
② Stable properties can be stored for a long time.
③ The adhesive of the coated transfer paper is relatively stable and can be stored for a long time.
④ The transfer rate of the coated transfer paper is greater than 85%, and the transferred patterns have bright colors and high precision.
⑤ When used in combination with CMC, it can reduce the cost of thermal sublimation coating and improve the drying time.
⑥ Increase the solid content of the thermal sublimation solution, reduce the viscosity of the coating, and the color of the transferred printing is bright.
Hot Tags: ultra-low viscosity cmc for thermal sublimation applications, China ultra-low viscosity cmc for thermal sublimation applications manufacturers, suppliers, factory, cmc purchase, cmc powder, cmc order, cmc for insulation, cmc outlook, cmc for building materials